ФОРМУВАННЯ КОНТАКТУ ПРИ ОДНООСЬОВОМУ ЗДАВЛЮВАННІ КРИСТАЛІЧНИХ ТВЕРДИХ ТІЛ: МЕХАНІЗМ ЗАКЛЮЧНОЇ СТАДІЇ

М.А. ВОЛОСЮК · Scientific Bulletin of Civil Engineering · 2020

In the present work on the base of the analysis of the contact geometry variations under uniaxial compression of crystalline solids, the substance transfer mechanism was proposed and experimentally approved for the final stage of the process where as a result of contortion and embedding the rough edges, the two-dimensional system of pores is formed. After the pore formation, in the contact plane of the crystal there occur alternating areas occupied by prismatic loops with different signs, i.e. the areas with different dilatation signs alternate. Between these areas, chemical potential gradients occur, resulting in countercurrent flows of point defects: vacancies come from healed pores and vacancy loops, and interstitial atoms – from dissolving interstitial loops formed before and generated at present. These flows lead to recombination of different sign defects and corresponding dislocation loops, increasing the contact area width, pore healing, stress relaxation, and decreasing dislocation density at the contact zone

Cited by 0 works.

Authors