АНАЛІЗ МАТЕРІАЛІВ ДЛЯ ВИРОБНИЦТВА ЗАЛІЗОБЕТОННИХ ШПАЛ НА ЗАВОДАХ ЗБШ УКРАЇНИ
Олександр Валерійович Романенко · Scientific Bulletin of Civil Engineering · 2015
The basic characteristics of the materials used for the manufacture of concrete sleepers were determined. It is recommended to use portlandcement PC I-500N with an activity of at least 36-39 MPa after steaming and 38-43 MPa at the age of 2 days. It is recommended to use a fraction mix 5-20 mm of broken stone and eliminate the use of fractions mix 5-25 mm, as well as to accept for further research on separate dosing fractions 5-10 and 10-20 mm of broken stone, granite screenings and sand.