ДОВГОВІЧНОСТЬ МЕТАЛЕВИХ ДИМОВИХ І ВЕНТИЛЯЦІЙНИХ ТРУБ ЗА КРИТЕРІЯМИ МЕХАНІКИ РУЙНУВАННЯ

С.Н. Яровий, О. В. Ярова · Scientific Bulletin of Civil Engineering · 2021

Throughout the life cycle, metal chimneys and ventilation pipes are exposed to significant force and wind influences, as well as the action of aggressive high-temperature gases outside and inside the pipe. Determination of durability of metal and ventilation pipes according to the criteria of fracture mechanics based on the approaches of physics and mechanochemistry of metals is considered. According to the characteristics of crack resistance, it is possible to assess the residual life of pipes with damage detected during diagnosis. Processing the results of few cycle tests of the samples, we obtain basic information about the properties of the metal, the conditions and characteristics of the tests, the size of the cracks, the size of the plastic zone before and during the tests. Based on the test results of the samples, a diagram of the cyclic crack resistance and the value of the crack propagation velocity is constructed. The diagrams of cyclic crack resistance are approximated and the parameters of the curve of low cyclic crack resistance are set. The formulas for determining the durability of metal pipes under cyclic loading by integrating the kinetic equation of low-cycle metal damage are obtained.

Cited by 0 works.

Authors