О некоторых закономерностях старения бетонных смесей и бетонов на органических вяжущих на примере дегтебетонов

Валерій Іванович Братчун, Д В Гуляк, В. Л. Беспалов · Вестник Харьковского национального автомобильно-дорожного университета · 2008

It has been established that the basic technology factor for defining the intensity of tar concrete mixtures ageing is the manufacture temperature whose influences is 10 times more than the time of organic binders and mineral material mixing in asphalt concrete mixer. The standard value of the consolidation factor of tar concrete mixes prepared at temperatures above 130 C is not provided. The generalised dependence of tar concrete mixture ageing in the course of manufacture and thermostating in climatic chamber has been drawn up in accordance with transportation requirements to the packing place and in the course of the accelerated thermal ageing in climatic chamber IP-1 at 60 С. Depending on viscosity of coal tar the annual equivalent of accelerated ageing time corresponding to ageing time of tar concrete coverings under operating conditions is calculated. Service life of tar concrete covering to the device of superficial fine-layer coverings for example, with the use of cast emulsion-mineral mixes is defined.

Cited by 0 works.

Authors