Трибологические характеристики различных пар трения при артропластике крупных суставов
Б. Ш. Минасов, Л. Ш. Шустер, Якупов Расуль Радикович et al. · Медицинский вестник Башкортостана · 2013
16 pairs of friction of hip prostheses have been studied in biological environment and dry friction conditions. In samples with a polyethylene liner the strength of adhesive bonds and the coefficient of friction were minimal in terms of the biological environment and increased at dry friction. In samples with a metal liner a friction coefficient reached the maximum value in a biological environment and reduced at dry friction. Optimal pairs of friction were oxinium-polyethylene and aluminum ceramics-polyethylene with the head of larger diameter (32mm), which showed a minimal coefficient of friction (0.009... 0.010), the lowest strength of adhesive bonds (0.2 MPa) and the lowest rate of hardening these bonds (0.006... 0.008).